WELDING CONSUMABLES

BROWSE

There are 4 key factors in contact tip manufacturing…

  1. GD&T – Bore / O.D. / Thread
  2. Surface finishes
  3. Metallurgical Composition
  4. Copper Heat Treated Condition

BRANDS AVAILABLE

BOB’S PRO TIP

There are a number of factors related the premature failure of a contact tip. There’s a 45-minute presentation in the video section of this website which has the information on conducting your company’s internal contact tip failure audit.

Contact Bob at Elite Welding Solutions for an appointment to review your welding challenges. bob@eliteweldingsolutions.com – 226-387-4541.